Título : Coprocessing of cellulose II with amorphous silicon dioxide: effect of silicification on the powder and tableting properties
Autor : Rojas Camargo, John Jairo
Kumar, Vijay
metadata.dc.subject.*: Celulosa - Química
Cellulose - Chemistry
Composición de Medicamentos - métodos
Drug Compounding - methods
Excipientes - Química
Excipients - Chemistry
Tamaño de la Partícula
Particle Size
Polvos - Química
Powders - Chemistry
Dióxido de Silicio - Química
Silicon Dioxide - Chemistry
Comprimidos - Química
Tablets - Chemistry
Fecha de publicación : 2012
Editorial : Taylor and Francis
Citación : Rojas J, Kumar V. Coprocessing of cellulose II with amorphous silicon dioxide: effect of silicification on the powder and tableting properties. Drug Dev Ind Pharm. 2012 Feb;38(2):209-26. doi: 10.3109/03639045.2011.597400.
Resumen : ABSTRACT: Aim: In recent years, coprocessing has been the most successful approach to improve and correct the functionality of excipients. The aim of this study is to coprocessed cellulose II with SiO(2) and to evaluate the resulting powder and tableting properties. Methods: Novel cellulose II:SiO(2) (98:2, 95:5, 90:10 and 80:20 w/w ratios) composites were produced by spray drying, wet granulation and spheronization techniques and the resulting powder and tableting properties were assessed. Results: Cellulose II:SiO(2) composites produced by spray- drying exhibited spherical/oblongate shape, narrow distribution and mean diameter from 51 to 75 µm. The composites produced by wet granulation had larger distribution, granular shape and a mean diameter from 105 to 129 µm. The spheronized composites showed the highest size (from 148 to 450 µm) and round shape. Bulk and tap densities and flow were reduced as the silicification level increased in the spray dried and wet granulated materials. Likewise, silicification increased the true density, porosity and surface roughness of these materials. Water sorption decreased only at silicification level of 20% being comparable to the ones shown by Prosolv(®) samples. Contact angles of all cellulose II materials were lower than those of cellulose I except for Celphere203 indicating better wettability. A 5% and 10% silicification levels rendered the strongest compacts for the spray dried and wet granulated materials, respectively. Silicification did not affect the fast disintegration properties of MCCII. Conclusions: Coprocessing proved to be useful tool to modify the powder and tableting properties of cellulose II.
metadata.dc.identifier.eissn: 1520-5762
ISSN : 0363-9045
metadata.dc.identifier.doi: 10.3109/03639045.2011.597400
Aparece en las colecciones: Artículos de Revista en Farmacéutica y Alimentarias

Ficheros en este ítem:
Fichero Descripción Tamaño Formato  
RojasJohn_2012_Coprocessing-Cellulose.pdfArtículo de investigación3.43 MBAdobe PDFVisualizar/Abrir


Este ítem está sujeto a una licencia Creative Commons Licencia Creative Commons Creative Commons